Home
Categories
EXPLORE
True Crime
Comedy
Business
Society & Culture
History
Sports
Health & Fitness
About Us
Contact Us
Copyright
© 2024 PodJoint
00:00 / 00:00
Sign in

or

Don't have an account?
Sign up
Forgot password
https://is1-ssl.mzstatic.com/image/thumb/Podcasts122/v4/de/d5/e0/ded5e03d-e8f2-a211-554c-3c1b56e7cdc9/mza_5288299469244869182.jpg/600x600bb.jpg
Casting Class
Batesville Products
35 episodes
4 days ago
An engineer's guide to manufacturing aluminum castings, hosted by Batesville Products, Inc. BPI has over 75 years of experience engineering, tooling, casting, machining, inspecting, and polishing aluminum and zinc products for 70 industries nationwide. Check out more content like videos, written guides, and case studies on our website: batesvilleproducts.com
Show more...
Business
RSS
All content for Casting Class is the property of Batesville Products and is served directly from their servers with no modification, redirects, or rehosting. The podcast is not affiliated with or endorsed by Podjoint in any way.
An engineer's guide to manufacturing aluminum castings, hosted by Batesville Products, Inc. BPI has over 75 years of experience engineering, tooling, casting, machining, inspecting, and polishing aluminum and zinc products for 70 industries nationwide. Check out more content like videos, written guides, and case studies on our website: batesvilleproducts.com
Show more...
Business
https://d3t3ozftmdmh3i.cloudfront.net/production/podcast_uploaded_nologo/24104496/24104496-1651504878076-fafd7304676d7.jpg
Prevent 10 Casting Defects
Casting Class
13 minutes 6 seconds
1 year ago
Prevent 10 Casting Defects

10 types of defects, what went wrong, and what you and your supplier can do to fix it together.

Chapters:

  1. Gas hole porosity
  2. Hydrogen gas porosity
  3. Inclusions
  4. Part design related defects
  5. Mold design related defects
  6. Mold maintenance related defects
  7. Supplier related defects

Defects include: porosity, hydrogen gas porosity, inclusions, shrink, bent, misrun, crack, rough surface finish, flash, and parting line shift.

Casting Class
An engineer's guide to manufacturing aluminum castings, hosted by Batesville Products, Inc. BPI has over 75 years of experience engineering, tooling, casting, machining, inspecting, and polishing aluminum and zinc products for 70 industries nationwide. Check out more content like videos, written guides, and case studies on our website: batesvilleproducts.com